Choose a material

Roofing sheets

Blachy trapezowe

Sandwich panels

Płyty warstwowe

PIR insulation boards

Płyty izolacyjne PIR

XPS

Izolacja XPS

Accessories

Akcesoria montażowe

Fencing

Sztachety metalowe

When does termPIR WS suit a flat roof?

PIR insulation

At a glance

Choose termPIR WS together with the waterproofing and fixing method for the flat roof. The rigid PIR core is faced on both sides with gas-permeable glass fleece, not gas-tight aluminium laminate. What adheres to one surface may not suit the other. Ask for documented compatibility of the deck, board, bonding or fixing layer and covering. At the outset, agree how the insulation will be supported around outlets, how locally reduced thickness at a parapet will be assessed, and who will protect the exposed roof if work stops before the waterproofing is complete.

termPIR WS insulation board showing its PIR core and facing

Specify the complete roof build-up

List the fleece-faced board, fixing layer and waterproofing in the enquiry. Request evidence for their combination before boards are spread over the roof. The core material does not determine surface adhesion.

Inspect the board joints and terminations on a garage roof before the final covering conceals them. Photograph the outlets and agree who keeps rain out during interruptions. An insulated deck is not yet a waterproof roof.

Detail the joints at outlets

WS is available with square or profiled edges. Check the label and confirm that neighbouring boards fit on a stable surface without lifting an edge.

Lay out the last row between the outlet and service enclosure. Mark support for each short piece and retain access to form the outlet flashing. A factory edge does not support a curved offcut.

Conductivity where the roof narrows

Read the WS thickness bands: λ is 0.027 W/(m·K) below 80 mm, 0.026 from 80 to under 120 mm and 0.025 from 120 to 250 mm.

At a low parapet mark the reduced thickness on the section and use the conductivity for that dimension. Neither the average roof depth nor the best value in the table describes this restriction.

Keeping the fleece dry

Include the open edge in the end-of-day weather check. Glass fleece does not shed rain like finished waterproofing; the roof covering remains a separate layer.

Direct runoff from temporary protection away from installed boards. After a break check dryness and fleece condition before laying the membrane. Record the condition at handover between trades.

Service traffic, equipment and fire

For WS, record CS(10/Y)120 and the board’s reaction to fire: F at 20–49 mm, E at 50–250 mm. These do not classify the roof assembly.

On the plan distinguish the maintenance route from a stationary equipment foot. Indicate protection and load distribution for each. CS120 does not give an allowable permanent pressure; assess fire requirements for the specified roof separately.

Compare installed roof prices

List format, thickness, edge and interface with the covering alongside WS on the order. Name the specific adhesive or fixing if the system requires one.

Compare only fixing methods suitable for the roof. Price boards by cover area, fasteners or adhesive, deck preparation, penetrations and perimeter work. The total should buy a closed roof, not insulation left exposed.

7 branches. Materials closer to your project.

  • SEROCK — Dzierżenin 34 E [mapa]
  • BŁONIE — ul. Sochaczewska 138A [mapa]
  • RADOM — ul. Grobickiego 8 [mapa]
  • ŁÓDŹ — Natolin 8 [mapa]
  • OLSZTYN — Barczewo, ul. Prosta 9 [mapa]
  • WROCŁAW — ul. Jerzmanowska 10C [mapa]
  • GORZÓW WLKP. — ul. Zielona 33/34 [mapa]
Budowlanka.org — map

Free quote

What to include in your enquiry

Tell us how you plan to use the material, the dimensions and the quantity you need. Include the thickness, grade or variant name, along with the delivery town or your preferred collection branch. For a specific product, add its name or a link to the product page. We will reply to the email address you provide to discuss availability and the terms of your order.

More from the building guide